Bug-O WHEEL - KBUG-1036 125 Amp A: Oxidation tint (heat discoloration)
Description
A: Oxidation tint (heat discoloration) on the weld bead or adjacent HAZ is caused by chromium oxide forming at elevated temperature in the presence of atmospheric oxygen